| Category: | PUR-Eth,aliphat , Polyurethane (Polyether, Aliphatic) |
| Manufacturer: | Anderson Development Company |
| Trademark: | Andur |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | 3ExWHX_Andur-AL-80-5-AP-Curene-110.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
| Andur AL80-5AP is a polyether (PTMG) based prepolymer terminated with an aliphatic isocyanate to improve color stability, hydrolytic stability, and give longer pot life. |
| General Information | |
|---|---|
| Features |
|
| Forms |
|
| Hardness | Nominal Value | Test Method | |
|---|---|---|---|
| Durometer Hardness (Shore A) | 83 | ASTM D2240 |
| Elastomers | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Stress | ASTM D412 | ||
| 100% strain | 5.38 | MPa | ASTM D412 |
| 300% strain | 13.9 | MPa | ASTM D412 |
| Tensile Strength (Yield) | 42.7 | MPa | ASTM D412 |
| Tensile Elongation (Break) | 430 | % | ASTM D412 |
| Compression Set | 52 | % | ASTM D395B |
| Bayshore Resilience | 40 | % | ASTM D2632 |
| Thermoset | Nominal Value | Unit | |
|---|---|---|---|
| Pot Life | 8.0 | min | |
| Demold Time (100°C) | 30 | min | |
| Post Cure Time | |||
| 21°C | 72 | hr | |
| 100°C | 16 | hr |
| Additional Information |
|---|
| Die C Tear, ASTM D1004: 350 pliAverage Split Tear, ASTM D1938: 100 pliStoichiometry Curative Level: 95%Mix Temperature: Andur AL 80-5 AP: 158°F Curene 110: 72°F |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| RTP 300 TFE 15 FR | RTP Company | PC | RTP |
| apilon 52® TLE 25 | API SpA | TPU-Polyether | apilon 52® |
| Cri-Line LC-715 | Cri-Tech, Inc. | Fluorelastomer | Cri-Line |
| Dynaflex™ G7630-1 (Natural) | PolyOne Corporation | TPE | Dynaflex™ |
| Elastollan® 880A-13N | BASF Corp. Thermoplastic Polyurethanes | TPU-Polyester | Elastollan® |