| Category: | PP Impact Copolymer , Polypropylene Impact Copolymer |
| Manufacturer: | Safripol (PTY) LTD |
| Trademark: | Safron® |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | 2tVqPD_Safron-C770-70RNA.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
|
Safron® C770-70RNA Polypropylene Resin is a high performance impact copolymer developed especially for high speed thin wall injection moulding. It is a very high melt flow rate impact copolymer featuring good impact strength. Safron® C770-70RNA Polypropylene Resin is designed and formulated to allow for easy processing, short cycle times, and good part dimensional stability. Safron® C770-70RNA Polypropylene Resin contains an effective anti-static package. |
| General Information | |
|---|---|
| Additive |
|
| Features |
|
| Uses |
|
| Agency Ratings |
|
| Processing Method |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Density | 0.900 | g/cm³ | ISO 1183 |
| Melt Mass-Flow Rate (MFR) (230°C/2.16 kg) | 70 | g/10 min | ISO 1133 |
| Hardness | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Durometer Hardness (Shore D, Injection Molded) | 60 | ISO 868 |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Stress (Yield, Injection Molded) | 21.0 | MPa | ISO 527-2 |
| Tensile Strain (Yield, Injection Molded) | 5.0 | % | ISO 527-2 |
| Flexural Modulus (Injection Molded) | 1050 | MPa | ISO 178 |
| Impact | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Charpy Notched Impact Strength | ISO 179/1eA | ||
| -20°C, injection molding | 4.2 | kJ/m² | ISO 179/1eA |
| 0°C, injection molding | 5.0 | kJ/m² | ISO 179/1eA |
| 23°C, injection molding | 7.5 | kJ/m² | ISO 179/1eA |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Heat Deflection Temperature 1(0.45 MPa, Unannealed) | 70.0 | °C | ISO 75-2/B |
| Vicat Softening Temperature 2 | 146 | °C | ISO 306/A |
| Injection | Nominal Value | Unit | |
|---|---|---|---|
| Rear Temperature | 190 | °C | |
| Middle Temperature | 220 - 240 | °C | |
| Front Temperature | 240 - 260 | °C | |
| Nozzle Temperature | 240 | °C |
| Injection instructions |
|---|
| Zone 4 Temperature: 260°C |
| Note Message | |
|---|---|
| 1 . | Injection Molded |
| 2 . | Injection Molded |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| Braskem PE SHE150 | Braskem | HDPE | Braskem PE |
| FERREX® GPP40CF | Ferro Corporation | PP, Unspecified | FERREX® |
| Kazan LDPE 153-11K | Kazanorgsintez Joint Stock Company | LDPE | Kazan LDPE |
| Karina MBPEB WHITE -E 1000/0085-IE | Karina Ind. e Com. de Plásticos Ltda | PVC, Unspecified | Karina |
| Petrotene® PP A3 E8 CNZ0018 PH346 MSP | Petropol Industry and Trade of Polymers LTDA | PP Homopolymer | Petrotene® PP |