Category: | PP Impact Copolymer , Polypropylene Impact Copolymer |
Manufacturer: | Braskem Europe GmbH |
Trademark: | Braskem PP |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | 2gazZ1_Braskem-PP-C113-01.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
Braskem C113-01 Polypropylene Impact Copolymer is a high performance impact copolymer developed for sheet extrusion and blow moulding applications. Main Characteristics:
Complies with:
Applications:
|
General Information | |
---|---|
Agency Ratings |
|
Forms |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Density | 0.900 | g/cm³ | ISO 1183 |
Melt Mass-Flow Rate (MFR) (230°C/2.16 kg) | 0.90 | g/10 min | ISO 1133 |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Stress (Yield, Injection Molded) | 24.0 | MPa | ISO 527-2 |
Tensile Strain (Yield, Injection Molded) | 15 | % | ISO 527-2 |
Flexural Modulus (Injection Molded) | 1100 | MPa | ISO 178 |
Impact | Nominal Value | Unit | Test Method |
---|---|---|---|
Charpy Notched Impact Strength | ISO 179/eA | ||
0°C, Injection Molded | 12 | kJ/m² | |
23°C, Injection Molded | 60 | kJ/m² |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Heat Deflection Temperature (0.45 MPa, Unannealed) | 85.0 | °C | ISO 75-2/B |
Vicat Softening Temperature | 146 | °C | ISO 306/A |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
TechnoDur PBT 4 GF10 black (9992) | TechnoCompound GmbH | PBT | TechnoDur |
KOPA® KN173MC | Kolon Plastics, Inc. | Nylon 6 | KOPA® |
Jackdaw PP EW13NT6459 | Jackdaw Polymers | PP, Unspecified | Jackdaw PP |
Polyrocks 7001D | Polyrocks Chemical Co., Ltd | ABS | Polyrocks |
LEXAN™ HFD4413 resin | SABIC Innovative Plastics Asia Pacific | PC | LEXAN™ |