| Category: | TPE , Thermoplastic Elastomer |
| Manufacturer: | Teknor Apex Company |
| Trademark: | Monprene® |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | 2Zh3BV_Monprene-CP-22147.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
| Monprene CP-22147 is a clear thermoplastic elastomer designed for a variety of consumer product applications requiring a soft, rubber-like feel. Monprene CP-22147 is an ozone resistant grade that exhibits excellent good abrasion resistance and is suitable for injection molding and extrusion. |
| General Information | |
|---|---|
| Features |
|
| Uses |
|
| Appearance |
|
| Forms |
|
| Processing Method |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Specific Gravity | 0.888 | g/cm³ | ASTM D792 |
| Melt Mass-Flow Rate (MFR) (200°C/5.0 kg) | 1.5 | g/10 min | ASTM D1238 |
| Hardness | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Durometer Hardness | ASTM D2240 | ||
| Shaw A | 52 | ASTM D2240 | |
| Shaw A, 5 seconds | 50 | ASTM D2240 |
| Elastomers | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Stress | ASTM D412 | ||
| 100% strain | 1.83 | MPa | ASTM D412 |
| 200% strain | 2.83 | MPa | ASTM D412 |
| 300% strain | 4.14 | MPa | ASTM D412 |
| Tensile Strength (Break) | 13.8 | MPa | ASTM D412 |
| Tensile Elongation (Break) | 640 | % | ASTM D412 |
| Tear Strength 1 | 43.8 | kN/m | ASTM D624 |
| Compression Set (23°C, 22 hr) | 13 | % | ASTM D395 |
| Injection | Nominal Value | Unit | |
|---|---|---|---|
| Rear Temperature | 182 - 232 | °C | |
| Middle Temperature | 188 - 238 | °C | |
| Front Temperature | 193 - 243 | °C | |
| Nozzle Temperature | 199 - 249 | °C | |
| Processing (Melt) Temp | 199 - 249 | °C | |
| Mold Temperature | 35.0 - 48.9 | °C | |
| Injection Pressure | 1.38 - 5.52 | MPa | |
| Injection Rate | Fast | ||
| Back Pressure | 0.172 - 0.689 | MPa | |
| Screw Speed | 50 - 100 | rpm | |
| Cushion | 3.81 - 25.4 | mm |
| Injection instructions |
|---|
| 无需干燥。但如果湿度过大,则将粒料在150°F (65°C)的温度下干燥2-4小时。 |
| Extrusion | Nominal Value | Unit | |
|---|---|---|---|
| Cylinder Zone 1 Temp. | 182 - 232 | °C | |
| Cylinder Zone 2 Temp. | 188 - 238 | °C | |
| Cylinder Zone 3 Temp. | 193 - 243 | °C | |
| Cylinder Zone 5 Temp. | 199 - 249 | °C | |
| Die Temperature | 199 - 249 | °C |
| Extrusion instructions |
|---|
| 螺杆转速30 - 100 rpm |
| Note Message | |
|---|---|
| 1 . | C mould |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| SOLPLAST TC 1000B | UTEKSOL d.o.o. | SBS | SOLPLAST TC |
| SureSpec IP-005NB | Genesis Polymers | PP Impact Copolymer | SureSpec |
| Vi-Chem PVC VNC87-30I | Vi-Chem Corporation | PVC, Unspecified | Vi-Chem PVC |
| HIPEX® HX6ICN (Series: HTR/OR) | KRAIBURG TPE | TPE | HIPEX® |
| LG ASA LI970HF | LG Chem Ltd. | ASA | LG ASA |