Category: | Nylon 6 , Polyamide 6 |
Manufacturer: | PENTAC Polymer GmbH |
Trademark: | PENTAMID B |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | 2RgGeS_PENTAMIDBGV10MC20H2LSblack.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
Normal viscosity, high heat stabilised polyamide 6, 10% glass fiber and 20% mineral reinforced, laser markable |
General Information | |
---|---|
Filler / Reinforcement |
|
Additive |
|
Features |
|
Agency Ratings |
|
Appearance |
|
Forms |
|
Processing Method |
|
Physical | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Density | 1.36 | -- | g/cm³ | ISO 1183 |
Molding Shrinkage | ISO 294-4 | |||
Transverse flow | 0.80 | -- | % | ISO 294-4 |
Flow | 0.50 | -- | % | ISO 294-4 |
Water Absorption | ISO 62 | |||
Saturated, 23°C | 6.7 | -- | % | ISO 62 |
Equilibrium, 23°C, 50% RH | 2.1 | -- | % | ISO 62 |
Viscosity Number | 145 | -- | cm³/g | ISO 307 |
Mechanical | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Tensile Modulus | 8200 | 5700 | MPa | ISO 527-2/1 |
Tensile Stress (Break) | 110 | 70.0 | MPa | ISO 527-2/5 |
Tensile Strain (Break) | 3.5 | 4.5 | % | ISO 527-2/5 |
Impact | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Charpy Notched Impact Strength (23°C) | 5.0 | 8.0 | kJ/m² | ISO 179/1eA |
Charpy Unnotched Impact Strength (23°C) | 45 | 65 | kJ/m² | ISO 179/1eU |
Thermal | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Heat Deflection Temperature | ||||
0.45 MPa, not annealed | 220 | -- | °C | ISO 75-2/B |
1.8 MPa, not annealed | 200 | -- | °C | ISO 75-2/A |
Melting Temperature | 222 | -- | °C | ISO 11357-3 |
Flammability | Dry | Conditioned | Test Method | |
---|---|---|---|---|
Flame Rating | UL 94 | |||
1.6 mm | HB | -- | UL 94 | |
3.2 mm | HB | -- | UL 94 |
Additional Information | Dry | Conditioned | Test Method | |
---|---|---|---|---|
ISO Shortname | PA6, MHRC, 14-080, GF10+MD20 X | -- | ISO 1874 |
Injection | Dry | Unit | |
---|---|---|---|
Drying Temperature | 80 | °C | |
Drying Time | 4.0 | hr | |
Suggested Max Moisture | 0.050 - 0.13 | % | |
Suggested Max Regrind | 20 | % | |
Rear Temperature | 265 - 280 | °C | |
Middle Temperature | 275 - 300 | °C | |
Front Temperature | 280 - 290 | °C | |
Processing (Melt) Temp | 260 - 300 | °C | |
Mold Temperature | 40 - 60 | °C | |
Injection Pressure | 72.0 | MPa | |
Screw L/D Ratio | 18.0:1.0 to 22.0:1.0 | ||
Screw Compression Ratio | 2.2:1.0 to 2.8:1.0 |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
Prop 6003 | Putsch Kunststoffe GmbH | PP, Unspecified | Prop |
RTP 4405 FR L | RTP Company | Nylon, Unspecified | RTP |
QR Resin QR-1310IM-GF30 | QTR, Inc. | PC+Polyester | QR Resin |
Resirene READ 9500 RAF | Resirene, S.A. de C.V. | PS (HIPS) | Resirene |
NYLOY® NG-0033N-V0 | Nytex Composites Co., Ltd. | Nylon 6 | NYLOY® |