| Category: | TPU-Polyester , Thermoplastic Polyurethane Elastomer (Polyester) |
| Manufacturer: | ResMart |
| Trademark: | ResMart Ultra |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | 2CXqGM_ResMart-Ultra-TPU-85A-ES.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
| Polyester based TPU Shore 85A hardness for injection molding or extrusion applications |
| General Information | |
|---|---|
| Agency Ratings |
|
| RoHS Compliance |
|
| Processing Method |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Specific Gravity | 1.19 | g/cm³ | ASTM D792 |
| Hardness | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Durometer Hardness (Shore A) | 85 | ASTM D2240 |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Strength | 31.0 | MPa | ASTM D638 |
| Elastomers | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Elongation (Break) | 520 | % | ASTM D412 |
| Tear Strength | 100 | kN/m | ASTM D624 |
| Flammability | Nominal Value | Test Method | |
|---|---|---|---|
| Flame Rating | HB | UL 94 |
| Injection | Nominal Value | Unit | |
|---|---|---|---|
| Drying Temperature - Desiccant Dryer | 90.0 to 100 | °C | |
| Drying Time - Desiccant Dryer | 3.0 to 4.0 | hr | |
| Suggested Max Moisture | 0.010 | % | |
| Processing (Melt) Temp | 191 to 204 | °C |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| Fainplast PVC FKA 85 | Fainplast Compounds S.r.l | PVC, Unspecified | Fainplast PVC |
| Fainplast PVC PM 5526/1 | Fainplast Compounds S.r.l | PVC, Flexible | Fainplast PVC |
| INEOS PP 240-CA12 | INEOS Olefins & Polymers Europe | PP Random Copolymer | INEOS PP |
| Polifor® E 8 TR/30 UV GRIGIO 7061 (648) | SO.F.TER. SPA | PP Copolymer | Polifor® |
| Sylvin 8205-75UV Brown 7469 | Sylvin Technologies Incorporated | PVC, Unspecified | Sylvin |