Category: | Acetal (POM) Homopolymer , Acetal (POM) Homopolymer |
Manufacturer: | Techmer Engineered Solutions |
Trademark: | Plaslube® |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | 1wt3GX_Plaslube-AC-81-TF-20-Natl.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
Acetal Homopolymer is the specific generic type. |
General Information | |
---|---|
Additive |
|
Features |
|
RoHS Compliance |
|
Appearance |
|
Forms |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Specific Gravity | 1.53 | g/cm³ | ASTM D792 |
Molding Shrinkage - Flow | 2.2 | % | ASTM D955 |
Water Absorption (24 hr) | 0.23 | % | ASTM D570 |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Strength (Yield) | 58.6 | MPa | ASTM D638 |
Flexural Modulus | 2690 | MPa | ASTM D790 |
Flexural Strength (Yield) | 82.7 | MPa | ASTM D790 |
Impact | Nominal Value | Unit | Test Method |
---|---|---|---|
Notched Izod Impact (23°C, 3.18 mm) | 48 | J/m | ASTM D256 |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Deflection Temperature Under Load (1.8 MPa, Unannealed) | 132 | °C | ASTM D648 |
Injection | Nominal Value | Unit | |
---|---|---|---|
Drying Temperature | 71.1 | °C | |
Drying Time | 2.0 | hr | |
Rear Temperature | 177 to 193 | °C | |
Middle Temperature | 188 to 210 | °C | |
Front Temperature | 182 to 199 | °C | |
Nozzle Temperature | 177 to 204 | °C | |
Processing (Melt) Temp | 193 to 216 | °C | |
Mold Temperature | 82.2 to 121 | °C | |
Injection Rate | Moderate | ||
Back Pressure | 0.00 to 0.172 | MPa | |
Screw Speed | 70 to 80 | rpm |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
Texin® 1210 | Covestro - PUR | TPU-Polyester | Texin® |
Arlon® AD255 | Arlon-MED | PTFE | Arlon® |
Emulprene® 261 | INSA | SBR, Emulsion | Emulprene® |
INSPIRE™ 227 | Braskem Europe GmbH | PP, Unspecified | INSPIRE™ |
Lumid® GP3400A(W) | LG Chem Ltd. | Nylon 6 | Lumid® |