Monprene RG-10140 is specifically designed for regulated applications including food contact, toys, and children's products. This grade is suitable for injection molding. Monprene RG-10140 complies with various US FDA and European regulations and directives for food contact and toy safety. Please contact Teknor Apex for a regulatory compliance letter.
General Information
Features
  • Low Specific Gravity
  • Without Fillers
  • Low density
  • smoothness
  • Low liquidity
  • Lubrication
  • Compliance of Food Exposure
  • BPA-free
  • No kinetic components
  • Hardness, low
Uses
  • Cosmetic Packaging
  • Kitchen utensils
  • Non-specific food applications
  • Cover
  • Food packaging
  • Food service sector
  • Food container
  • Toys
  • Consumer goods application field
Agency Ratings
  • FDA Food Exposure, Not Rated
  • European food contact, not rated
Appearance
  • Translucent
Forms
  • Particle
Processing Method
  • Injection molding
PhysicalNominal ValueUnitTest Method
Specific Gravity 0.888g/cm³ISO 1183
Melt Mass-Flow Rate (MFR) (200°C/5.0 kg)8.0g/10 minASTM D1238
HardnessNominal ValueUnitTest Method
Durometer Hardness (Shore A, 5 sec)40ISO 868
ElastomersNominal ValueUnitTest Method
Tensile Stress - Across Flow (100% Strain)0.500MPaISO 37
Tensile Stress - Across Flow (Break)5.00MPaISO 37
Tensile Elongation - Across Flow (Break)860%ISO 37
Tear Strength 1ISO 34-1
    Transverse flow 8.3kN/mISO 34-1
    Flow 14kN/mISO 34-1
Compression Set 2(70°C, 22 hr)23%ISO 815
Fill AnalysisNominal ValueUnitTest Method
Apparent Viscosity (200°C, 206 sec^-1)214Pa·sASTM D3835
Legal statement
The information and recommendations contained in this bulletin are, to the best of our knowledge, accurate and reliable but no guarantee of their accuracy is made. All products are sold upon condition that purchasers shall make their own tests to determine the suitability of such products for their particular purposes and uses and purchaser assumes all risks and liability for the results of use of the products, including use in accordance with seller's recommendations. Nothing in this bulletin constitutes permission or a recommendation to practice or use any invention covered by any patent owned by this company or others. There is no warranty of merchantability and there are no other warranties for the products described. For detailed Product Stewardship information, please contact us. Any product of Teknor Apex, including product names, shall not be used or tested in medical or food contact applications without the prior written acknowledgement of Teknor Apex as to the intended use. Please note that some products may not be available in one or more countries.
InjectionNominal ValueUnit
Rear Temperature 160 - 177°C
Middle Temperature 182 - 204°C
Front Temperature 193 - 216°C
Nozzle Temperature 182 - 227°C
Processing (Melt) Temp 182 - 227°C
Mold Temperature 26.7 - 48.9°C
Injection Rate Moderate-Fast
Back Pressure 0.172 - 0.689MPa
Screw Speed 50 - 100rpm
Cushion 3.81 - 12.7mm
Injection instructions
Drying is not necessary. However, if moisture is a problem, dry the pellets for 2 to 4 hours at 150°F (65°C).
Note Message
1 .Method B, right-angle specimen (without cut)
2 .Type a
Resin Grade Manufacturer Category Trademark
Boda BDT246-1EP Chenguang Fluoro & Silicone Elastomers Co., Ltd. Fluorelastomer Boda
ExxonMobil™ PP7555KNE2 ExxonMobil Chemical PP Impact Copolymer ExxonMobil™
ESENTTIA 08H85-1 Polipropileno del Caribe S.A. PP Homopolymer ESENTTIA
Hostalen CRP 100 RD black LyondellBasell Industries HDPE Hostalen
LIHAN® P601EX Nanjing Lihan Chemical Co., Ltd. PP, Unspecified LIHAN®