| Category: | TPO , Compounded Polypropylene |
| Manufacturer: | Technovinyl Polymers India Ltd. |
| Trademark: | K PP |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | 1dsDlZ_K-PP-7072.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
|
K PP 7072 is a Compounded Polypropylene material. It is available in Africa & Middle East. Important attributes of K PP 7072 are:
Typical application of K PP 7072: Automotive |
| General Information | |
|---|---|
| Features |
|
| Uses |
|
| Appearance |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Specific Gravity | 0.990 | g/cm³ | ASTM D792 |
| Melt Mass-Flow Rate (MFR) (230°C/2.16 kg) | > 7.0 | g/10 min | ASTM D1238 |
| Molding Shrinkage - Flow | < 1.0 | % |
| Hardness | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Rockwell Hardness (R-Scale) | 118 |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Strength (Yield) | 42.2 | MPa | ASTM D638 |
| Flexural Modulus | 2240 | MPa | ASTM D790 |
| Impact | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Notched Izod Impact (23°C) | 39 | J/m | ASTM D256 |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Deflection Temperature Under Load (0.45 MPa, Unannealed) | 140 | °C | ASTM D648 |
| Flammability | Nominal Value | Test Method | |
|---|---|---|---|
| Flame Rating | HB | UL 94 |
| Additional Information | Nominal Value | Unit | |
|---|---|---|---|
| Heat Resistance - Long Term | > 125 | °C |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| VESTAMID® Care ML16 | Evonik Industries AG | Nylon 12 | VESTAMID® Care |
| Electrafil® PC 04006 | Techmer Engineered Solutions | PC | Electrafil® |
| ELASTOSIL® R plus 4306/70 | Wacker Chemie AG | Silicone | ELASTOSIL® R plus |
| KetaSpire® KT-880 GF30 | Solvay Specialty Polymers | PEEK | KetaSpire® |
| PENTAMID A L1 H black | PENTAC Polymer GmbH | Nylon 66 | PENTAMID A |