| Category: | Nylon 6 , Polyamide 6 |
| Manufacturer: | Kolon Plastics, Inc. |
| Trademark: | KOPA® |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | 1THTTP_KOPAKN133G15BRN.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
| Dimensionally stable, Polyamide6 Compound resin |
| General Information | |
|---|---|
| Filler / Reinforcement |
|
| Features |
|
| RoHS Compliance |
|
| Processing Method |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Density | 1.24 | g/cm³ | ISO 1183 |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Stress (23°C) | 125 | MPa | ISO 527-2 |
| Tensile Strain (Break, 23°C) | 3.0 | % | ISO 527-2 |
| Flexural Modulus (23°C) | 5000 | MPa | ISO 178 |
| Flexural Stress (23°C) | 160 | MPa | ISO 178 |
| Impact | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Charpy Notched Impact Strength (23°C) | 7.5 | kJ/m² | ISO 179/1eA |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Heat Deflection Temperature (1.8 MPa, Unannealed) | 185 | °C | ISO 75-2/A |
| Melting Temperature | 225 | °C | ISO 11357-3 |
| Injection | Nominal Value | Unit | |
|---|---|---|---|
| Drying Temperature - Desiccant Dryer | 80 - 100 | °C | |
| Drying Time - Desiccant Dryer | 4.0 - 5.0 | hr | |
| Suggested Max Moisture | < 0.050 | % | |
| Rear Temperature | 230 | °C | |
| Middle Temperature | 240 | °C | |
| Front Temperature | 245 | °C | |
| Nozzle Temperature | 250 | °C | |
| Mold Temperature | 60 - 80 | °C |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| RTP 4282 TFE 10 | RTP Company | PI, TP | RTP |
| Medalist® MD-575D | Teknor Apex Company | TPE | Medalist® |
| Cawiton® CN960 | Wittenburg B.V. | SEBS | Cawiton® |
| Hylon® N2000 | Ravago Manufacturing Americas, LLC | Nylon 6 | Hylon® |
| PHOENIX™ 6602 | Phon Tech Industrial Company | TPE | PHOENIX™ |