Bergamid™ A70 G30 NC129

Category: Nylon 66 , Polyamide 66
Manufacturer: PolyOne Corporation
Trademark: Bergamid™
Fillers: -
Ports: Qinzhou, Shekou, Shanghai, Ningbo
Delivery Terms FOB, CIF, DAP, DAT, DDP
PDF: 0vkC26_Bergamid-A70-G30-NC129.pdf
PRICE: ​Order Products​ email   sales@su-jiao.com
Wechat: WECHAT
Message
Bergamid™A70 G30 NC129 is a polyamide 66 (nylon 66) product, which contains a 30% glass fiber reinforced material. It can be processed by injection molding and is available in the Asia-Pacific region.
General Information
Filler / Reinforcement
  • Glass fiber reinforced material, 30% filler by weight
Appearance
  • Natural color
Processing Method
  • Injection molding
PhysicalNominal ValueUnitTest Method
Density 1.36g/cm³ISO 1183
Molding Shrinkage - Flow 0.30 - 0.60%ASTM D955
MechanicalNominal ValueUnitTest Method
Tensile Stress 180MPaISO 527-2
Flexural Modulus 8500MPaISO 178
Flexural Stress 260MPaISO 178
ImpactNominal ValueUnitTest Method
Charpy Notched Impact Strength 12kJ/m²ISO 179
ThermalNominal ValueUnitTest Method
Deflection Temperature Under Load (1.8 MPa, Unannealed, 3.20 mm)245°CASTM D648
InjectionNominal ValueUnit
Drying Temperature 80.0 - 90.0°C
Drying Time 4.0 - 6.0hr
Rear Temperature 260 - 280°C
Middle Temperature 260 - 280°C
Front Temperature 260 - 280°C
Mold Temperature 65.0 - 85.0°C
Injection instructions
Injection Pressure: MED-HIGHHold Pressure: MED-HIGHScrew Speed: MODERATEBack Pressure: LOW
Resin Grade Manufacturer Category Trademark
RTP 201 UV RTP Company Nylon 66 RTP
Pro-fax EP501V LyondellBasell Industries PP Impact Copolymer Pro-fax
QR Resin QR-1310IM-GF30 QTR, Inc. PC+Polyester QR Resin
Thermylene® P-9900-0712 Asahi Kasei Plastics North America Inc. PP, Unspecified Thermylene®
Zytel® MT409AHS BK010 DuPont Performance Polymers Nylon 66 Zytel®