| Category: | Nylon 66 , Polyamide 66 |
| Manufacturer: | Wellman Engineering Resins |
| Trademark: | Wellamid® |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | 0UhBW8_Wellamid-GF33-66-XE-BKDX9.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
|
Wellamid® GF33-66 XE-BKDX9 is a Polyamide 66 (Nylon 66) material filled with 33% glass fiber. It is available in Asia Pacific, Europe, Latin America, or North America. Typical application of Wellamid® GF33-66 XE-BKDX9: Automotive |
| General Information | |
|---|---|
| Filler / Reinforcement |
|
| Forms |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Density | 1.40 | g/cm³ | ISO 1183 |
| Molding Shrinkage | ISO 294-4 | ||
| Across Flow : 23°C | 0.90 to 1.3 | % | |
| Flow : 23°C | 0.20 to 0.60 | % |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Stress (Yield, 23°C) | 180 | MPa | ISO 527-2 |
| Tensile Strain (Yield, 23°C) | 2.0 | % | ISO 527-2 |
| Flexural Modulus (23°C) | 8800 | MPa | ISO 178 |
| Flexural Stress (23°C) | 245 | MPa | ISO 178 |
| Impact | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Notched Izod Impact Strength (23°C) | 9.0 | kJ/m² | ISO 180 |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Heat Deflection Temperature (1.8 MPa, Unannealed) | 245 | °C | ISO 75-2/A |
| Melting Temperature (DSC) | 260 | °C | ISO 3146 |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| Maxelast® C4803 | Nantong Polymax Elastomer Technology, Co., Ltd | TPE | Maxelast® |
| TIPPLEN® H 681 F | MOL Petrochemicals Co. Ltd. | PP Homopolymer | TIPPLEN® |
| HiFill® POM CO 0167 S1 LE | Techmer Engineered Solutions | Acetal (POM) Copolymer | HiFill® |
| KOPA® KN173ST3R | Kolon Plastics, Inc. | Nylon 6 | KOPA® |
| Sylvin 4200-85 Brown 7442 | Sylvin Technologies Incorporated | PVC, Unspecified | Sylvin |