| Category: | TPU-Polyester , Thermoplastic Polyurethane Elastomer (Polyester) |
| Manufacturer: | Crosspolimeri S.p.A. |
| Trademark: | EFRHATAN |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | 0T0lKW_EFRHATAN-90.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
|
EFRHATAN : is the trade-mark of our modified polyurethane-polyesther suitable for sheath. EFRHATAN 90 : material suitable for sheathing extrusion on cables wire application. |
| General Information | |
|---|---|
| Uses |
|
| Forms |
|
| Processing Method |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Specific Gravity | 1.20 | g/cm³ | ASTM D792 |
| Hardness | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Shore Hardness (Shore A) | 89 | ASTM D2240 |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Stress (Yield) | 49.0 | MPa | IEC 60811 |
| Tensile Strain (Break) | 550 | % | IEC 60811 |
| Abrasion Resistance | 35.0 | mm³ | DIN 53516 |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Cold Flexibility | -22 | °C | ISO 458 |
| Exercise Temperature | 90 | °C | |
| Thermal Stability | > 1 | hr | ISO R 182 |
| Extrusion | Nominal Value | Unit | |
|---|---|---|---|
| Head Temperature | 200 | °C |
| Elastomers | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tear Strength | 90 | kN/m | DIN 53515 |
| Aging | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Change in Tensile Strength in Air (120°C, 168 hr) | < 30 | % | UL 1581 |
| Change in Tensile Strain at Break in Air (120°C, 168 hr) | < 30 | % | UL 1581 |
| Change in Tensile Stress | UL 1581 | ||
| 90°C, 168 hr, in ASTM #2 Oil | < 30 | % | |
| 121°C, 18 hr, in ASTM #2 Oil | < 30 | % | |
| Change in Tensile Strain at Break | UL 1581 | ||
| 90°C, 168 hr, in ASTM #2 Oil | < 30 | % | |
| 121°C, 18 hr, in ASTM #2 Oil | < 30 | % |
| Flammability | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Oxygen Index 1 | 22 | % | ASTM D2863 |
| Extrusion | Nominal Value | Unit | |
|---|---|---|---|
| Drying Temperature | 90.0 | °C | |
| Drying Time | 3.0 to 6.0 | hr | |
| Cylinder Zone 1 Temp. | 170 | °C | |
| Cylinder Zone 2 Temp. | 180 | °C | |
| Cylinder Zone 3 Temp. | 190 | °C | |
| Cylinder Zone 4 Temp. | 210 | °C | |
| Die Temperature | 190 | °C |
| Note Message | |
|---|---|
| 1 . | Indicative value |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| Milastomer™ W700B | Mitsui Chemicals America, Inc. | TPV | Milastomer™ |
| THERMOLAST® K TC4PAZ (Series: AD/PA) | KRAIBURG TPE | TPE | THERMOLAST® K |
| ARMAMID® PA School 20.2 | Poly Plastic | Nylon 6 | ARMAMID® |
| Flontech® FT-CARR15-1 | Guarniflon S.p.A. - Flontech Division | PTFE | Flontech® |
| NEOFLON™ AP-210 | DAIKIN AMERICA, INC. | PFA | NEOFLON™ |