Halogen free flame retardant TPE for Wire & Cable applications, with excellent elasticity |
General Information | |
---|---|
Features |
|
Uses |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Specific Gravity | 1.07 | g/cm³ | ASTM D792 |
Hardness | Nominal Value | Unit | Test Method |
---|---|---|---|
Durometer Hardness | ASTM D2240 | ||
Shaw A | 95 | ASTM D2240 | |
Shaw D | 40 | ASTM D2240 |
Elastomers | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Strength (Yield) | 13.0 | MPa | ASTM D412 |
Tensile Elongation (Break) | 410 | % | ASTM D412 |
Electrical | Nominal Value | Unit | Test Method |
---|---|---|---|
Volume Resistivity | > 1.0E+14 | ohms·cm | ASTM D257 |
Dielectric Strength | > 20 | kV/mm | ASTM D149 |
Flammability | Nominal Value | Unit | Test Method |
---|---|---|---|
Flame Rating (3.0 mm) | V-0 | UL 94 |
Extrusion | Nominal Value | Unit | |
---|---|---|---|
Drying Temperature | 80 - 90 | °C | |
Drying Time | 3.0 - 4.0 | hr |
Extrusion instructions |
---|
Hopper Temperature: 150 - 170 °CTransmission Temperature: 180 - 200 °CMeasurement Temperature: 200 - 230 °CDie Temperature: 190 - 220 °CMesh Temperature: 100 - 200 mesh |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
RTV-2 P-20B | Silicones, Inc. | Silicone Rubber, RTV-2 | RTV-2 |
Rhelon F2538H-01 | RheTech, Inc. | Nylon 66 | Rhelon |
Niplene V2 | Soredi S.p.a. | PP Homopolymer | Niplene |
Grilamid® XE 3915 | EMS-GRIVORY | Nylon 12 | Grilamid® |
Plaslube® PA6/6 T/AL20 HS | Techmer Engineered Solutions | Nylon 66 | Plaslube® |