Category: | Nylon 12 , Polyamide 12 |
Manufacturer: | Arkema |
Trademark: | Rilsan® |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | 0GATlk_Rilsan-MA-4411.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
Rilsan® MA 4411 is a Polyamide 12 (Nylon 12) product. It can be processed by extrusion, injection molding, or profile extrusion and is available in Africa & Middle East, Asia Pacific, Europe, Latin America, or North America. Typical application: Automotive. Characteristics include:
|
General Information | |
---|---|
Additive |
|
Features |
|
Forms |
|
Processing Method |
|
Multi-Point Data |
|
Physical | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Density | 1030 | 1030 | kg/m³ | ISO 1183 1 |
Melt volume-flow rate (235°C/2.16 kg) | 5.00 | -- | cm³/10min | ISO 1133 2 |
Water Absorption | ISO 62 3 | |||
Saturation | 1.2 | -- | % | |
Equilibrium | 0.65 | -- | % |
Mechanical | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Tensile modulus | 555 | 500 | MPa | ISO 527-2 4 |
Tensile Stress (Yield) | 29.0 | 27.0 | MPa | ISO 527-2 5 |
Tensile Strain (Yield) | 23 | 22 | % | ISO 527-2 6 |
Nominal strain at break | > 50 | > 50 | % | ISO 527-2 7 |
Impact | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Charpy notched impact strength | ISO 179/1eA 8 | |||
-30°C | 4.00 | 6.00 | kJ/m² | |
23°C | -- | No Break | ||
Charpy impact strength | ISO 179/1eU 9 | |||
-30°C | No Break | No Break | ||
23°C | No Break | No Break | ||
Puncture energy (-30°C) | -- | 53.0 | J | ISO 6603-2 10 |
Puncture - maximum force (-30°C) | -- | 4570 | N | ISO 6603-2 11 |
Thermal | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Deflection Temperature Under Load (1.8 MPa) | 41.0 | -- | °C | ISO 75-2 12 |
Melting Temperature 13 | 175 | -- | °C | ISO 11357-3 14 |
Flammability | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Burning Behav. at 1.6mm nom. thickn. (1.60 mm) | HB | -- | ISO 1210 15 | |
Burning Behav. at thickness h (3.20 mm) | HB | -- | ISO 1210 16 | |
Oxygen index | 20 | -- | % | ISO 4589-2 17 |
Note Message | |
---|---|
1 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
2 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
3 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
4 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
5 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
6 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
7 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
8 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
9 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
10 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
11 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
12 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
13 . | 10 °C/min |
14 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
15 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
16 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
17 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
RTP 201 UV | RTP Company | Nylon 66 | RTP |
RTP 203 A FR UV | RTP Company | Nylon 6 | RTP |
GAPEX® RPP30EU68HB | Ferro Corporation | PP Copolymer | GAPEX® |
HIPOLEN P® MA 3R | HIPOL A.D. | PP Homopolymer | HIPOLEN P® |
Ixef® HC-1022 | Solvay Specialty Polymers | PARA | Ixef® |