| Category: | PPS , Polyphenylene Sulfide |
| Manufacturer: | ALBIS PLASTIC GmbH |
| Trademark: | TEDUR® |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | 03Cotf_TEDUR-L-9107-1.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
|
TEDUR® L 9107-1 is a Polyphenylene Sulfide (PPS) product filled with 40% glass fiber. It can be processed by injection molding and is available in Asia Pacific, Europe, or North America. Typical application: Engineering/Industrial Parts. Characteristics include:
|
| General Information | |
|---|---|
| Filler / Reinforcement |
|
| Features |
|
| Uses |
|
| Agency Ratings |
|
| RoHS Compliance |
|
| Processing Method |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Density | 1.65 | g/cm³ | ISO 1183 |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Modulus | 14500 | MPa | ISO 527-2 |
| Tensile Stress (Break) | 180 | MPa | ISO 527-2 |
| Tensile Strain (Break) | 1.8 | % | ISO 527-2 |
| Flexural Modulus | 13500 | MPa | ISO 178 |
| Flexural Stress | 260 | MPa | ISO 178 |
| Flexural Strain at Flexural Strength | 2.2 | % | ISO 178 |
| Impact | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Charpy Unnotched Impact Strength | ISO 179/1eU | ||
| -- | 55 | kJ/m² | |
| -30°C | 55 | kJ/m² | |
| Unnotched Izod Impact Strength | 45 | kJ/m² | ISO 180/1U |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Heat Deflection Temperature (1.8 MPa, Unannealed) | 260 | °C | ISO 75-2/A |
| Electrical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Surface Resistivity | > 1.0E+15 | ohms | IEC 60093 |
| Flammability | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Flame Rating (0.750 mm) | V-0 | UL 94 | |
| Glow Wire Flammability Index (2.00 mm) | 960 | °C | IEC 60695-2-12 |
| Injection | Nominal Value | Unit | |
|---|---|---|---|
| Drying Temperature - Desiccant Dryer | 130 to 140 | °C | |
| Drying Time - Desiccant Dryer | 2.0 to 4.0 | hr | |
| Processing (Melt) Temp | 320 to 340 | °C | |
| Mold Temperature | > 140 | °C |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| RTP 2385 A | RTP Company | PUR, Unspecified | RTP |
| RJM EL701 | RJM International, Inc. | PP, Unspecified | RJM |
| Stylac™ IC39A | Asahi Kasei Chemicals Corporation | ABS | Stylac™ |
| KRYSTALGRAN™ PE193-100 | Huntsman Corporation | PUR-Eth,aliphat | KRYSTALGRAN™ |
| TECHNYL eXten® D 219CR V33 NATURAL | Solvay Engineering Plastics | Nylon 66/610 | TECHNYL eXten® |