| Category: | PP Impact Copolymer , Polypropylene Impact Copolymer |
| Manufacturer: | Braskem Europe GmbH |
| Trademark: | Braskem PP |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | 00a7EL_Braskem-PP-C7057-07-Injection-Molding-.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
|
Braskem C7057-07 Polypropylene Resin is a high impact copolymer developed for injection moulding applications. Applications for Braskem C7057-07 Polypropylene Resin:
Main Characteristics:
Complies with:
|
| General Information | |
|---|---|
| Agency Ratings |
|
| Forms |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Density | 0.900 | g/cm³ | ISO 1183 |
| Melt Mass-Flow Rate (MFR) (230°C/2.16 kg) | 7.0 | g/10 min | ISO 1133 |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Stress (Yield, Injection Molded) | 26.0 | MPa | ISO 527-2 |
| Tensile Strain (Yield, Injection Molded) | 10 | % | ISO 527-2 |
| Flexural Modulus (Injection Molded) | 1200 | MPa | ISO 178 |
| Impact | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Charpy Notched Impact Strength | ISO 179/1eA | ||
| -20°C, Injection Molded | 3.0 | kJ/m² | |
| 0°C, Injection Molded | 5.0 | kJ/m² | |
| 23°C, Injection Molded | 10 | kJ/m² |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Heat Deflection Temperature (0.45 MPa, Unannealed) | 88.0 | °C | ISO 75-2/B |
| Vicat Softening Temperature | 151 | °C | ISO 306/A |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| Medalist® MD-50153 NAT X (PRELIMINARY DATA) | Teknor Apex Company | TPE | Medalist® |
| Telcar® 90-E607B-75NT | Teknor Apex Company | EVA | Telcar® |
| COSMOPLENE® AZ564G | TPC, The Polyolefin Company (Singapore) Pte Ltd | PP Copolymer | COSMOPLENE® |
| Latilon 30D-V0 | LATI S.p.A. | PC | Latilon |
| Karina WHITE PVC COMPOUND 924D10/349-IS | Karina Ind. e Com. de Plásticos Ltda | PVC, Unspecified | Karina |